To get in between the teeth, you can use either a really fine brush, a gundam marker, or a wash (the wash probably being the most difficult of the three).

Before I started customizing, I read Jin Saotome's tutorials (jincustom.com) several times and purchased the brushes, paints, dremel, apoxie, etc... that he recommended. I didn't buy it all at once, but as I started to broaden my horizons w/customizing, I picked up the tools needed to accomplish what I wanted to do.

Here are some things I think are important to know, and some tricks I use:

-I don't think I can stress enough that the quality of your paint brushes and paint make a BIG difference.

-Don't use enamel paint on action figures! Enamel paint reacts with the soft plastic parts and causes them to have a tacky feeling. Acrylic paints are the way to go (Testors Model Master Acrylics, Testors Floquil Acrylics, P3 Formula, Vallejo, and Reaper paints are some of the most reputable paints to use).

-I think I get better results when I stir my paints, instead of shaking them. Of course, I suppose you could do both.

-I thin my paints with regular Windex, and I clean my brush regularly while painting with Windex. I know it sounds weird, but I promise the results are great.

-Speaking of thinning paints, not all need to be thinned, but you want them to be about the consistency of milk.

-Do not stick the bristles over half way in the paint. If you get paint around the base of the bristles, it's harder to clean and cause the paint to dry and clump up at the base, which messes up the form of the bristles.

-Paint lightly. You only want the tip of the brush to touch the surface and you don't want to leave paint streaks.

-Paint in multiple thin layers (painting in thin layers allows the details of the sculpts remain visible and prominent along with providing a more durable paint job), but make sure each layer is dry before painting the next layer. I use a hair dryer to speed the process up (about 20 seconds should do it). Preferably, use a blow dryer with the ability to blow cool air as well, as you don't want to paint on a hot surface.

-Wash the figure with plain dish soap (non-scented) and scrub the individual pieces with a toothbrush in order to get the seal coat off that is put on at the factory. This coat can cause the paint to rub off easily and is meant to act as a repellant of sorts. Of course, rinse and dry before painting.

-In order to prevent paint rub in the joints, which is the cause of frustration for most customizers, you can do a few different things: 1. You can dremel the joint in order that that it doesn't rub against whichever limb it's connected to. 2. You can apply a very thin layer of super glue over the joint, after it's been painted, but this can be tricky and if you're not careful, you can glue the joint together. 3. I came up with my own technique where I use an exacto knife to cut out a thin sliver of the limb where it's rubbing against the joint. You have to be careful to not cut too far though.

-People like to seal their figures with products like Testors Dullcote, but I refrain from sealing my figures as I've read numerous posts from other customizers saying that it reacts with the soft plastic on action figures in much the same way enamel paint does. It leaves a tacky feeling, as if the paint isn't fully dry. Neither enamel, nor sealant sprays should react this way with hard plastic though (great for weapons, and other bits that you are able to spray by themselves). Again, I've never used a sealant after hearing too many horror stories, but that might not be the case for everyone. I guess you could try it at your own risk, but I would test on a toy with soft plastic that you don't care for first, just to make sure. Also, make sure to follow the directions on the can of the sealant when using it. Otherwise, you can get an uneven coating and it won't look right.

-PATIENCE!! Patience is definitely needed as mistakes are made more frequently and the finished product shows when you rush things. Take your time.

Those are just some pointers I can think of off the top of my head in order to get the best results when customizing. It's easy to get discouraged if your first few customs don't turn out well, but with proper tools, preparation and patience, you should be able to get good results!

I hope that helps!
__________________


Nick TMNT Customs: 1988/2003 Inspired Custom Nick Turtles

My Customs' Facebook Page: Cole Customs
Cloud Strife is offline   Reply With Quote
Old 10-18-2012, 09:26 AM   #2
Discogod
Resolutely Analogue.
 
Discogod's Avatar
 
Join Date: Jul 2010
Location: Birmingham, UK
Posts: 1,707
Quote:
Originally Posted by Cloud Strife View Post
-People like to seal their figures with products like Testors Dullcote, but I refrain from sealing my figures as I've read numerous posts from other customizers saying that it reacts with the soft plastic on action figures in much the same way enamel paint does. It leaves a tacky feeling, as if the paint isn't fully dry. Neither enamel, nor sealant sprays should react this way with hard plastic though (great for weapons, and other bits that you are able to spray by themselves). Again, I've never used a sealant after hearing too many horror stories, but that might not be the case for everyone. I guess you could try it at your own risk, but I would test on a toy with soft plastic that you don't care for first, just to make sure. Also, make sure to follow the directions on the can of the sealant when using it. Otherwise, you can get an uneven coating and it won't look right.
I can't disagree with this enough. Sealing the figure not only protects the paintjob, it'll also preserve it over time - some paints can react with the air over time, fading or even changing colour. Even a light coat of sealer can prevent that. I've made 500+ customs over the years and always seal them (usually with either Humbrol matt spray or Citadel Purity Seal), and I've never had a problem with tackiness.

As long as the sealer's acrylic-based, there shouldn't be any issues. Obviously, following the directions is paramount.

And to completely contradict myself, I wouldn't use spray sealer on soft rubber parts (like capes), as the solvents in spray CAN react with the softer, rubbery plastic. For those parts, I usually use a thin coat of brush-on sealer (again, usually Humbrol).
Discogod is offline   Reply With Quote
Reply

Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT -6. The time now is 07:02 AM.


Powered by vBulletin® Version 3.8.7
Copyright ©2000 - 2026, vBulletin Solutions, Inc.